Scott:

It is USP grade zinc oxide, which usually runs 4-5 times the price of standard zinc oxide. I have tested it, it does work, and it does give a very high glossy finish. However, it does not like temps over cone 6. You do not state at what cone you will be firing, so there is no recommendations I can offer. Several zinc oxides available in the pottery biz: some work better at cone 10, and others at cone 6. Perhaps a bit more info first.

Nerd