Hi all,

 

I'm just in love with this look and wonder how it's achieved: with underglaze over a white glaze? dipping a powdered (undiluted) mason stain over the wet white glaze? with drops of water on underglaze applied over wet white glaze? a cobalt oxide wash? Anyone??
Thanks! :)

post-11816-0-38806100-1461608387_thumb.jpg

post-11816-0-46046400-1461608522_thumb.jpg

post-11816-0-38806100-1461608387_thumb.jpg

post-11816-0-46046400-1461608522_thumb.jpg

Share this post


Link to post
Share on other sites

Diffusion. Look up Mocha Diffusion and you will read about the general technique. It looks like they likely used cobalt carbonate with vinegar applied to wet slip. I like this technique too. Looks like the banding wheel may have been used for the edge. There actually is a water colour effect but it involves highly toxic materials. 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.