Hello,

I would like to work with engobes. Can someone share his/her experience? With possible samples, formulas, etc...

I work normaly with electric skilll, but can use a gaze one also.

What are the colour possibilities, what receipts are trustable?

Greetings from Belgium

Share this post


Link to post
Share on other sites

Hello,

I would like to work with engobes. Can someone share his/her experience? With possible samples, formulas, etc...

I work normaly with electric skilll, but can use a gaze one also.

What are the colour possibilities, what receipts are trustable?

Greetings from Belgium

 

 

If you cannot buy your coloured engobes you can mix

50 % half fat clay

50% calcined kaolin

+ coloured stain

+ a little CMC for bonding

 

this goes also for high fire temperatures.

Enjoy

Judith - autour de la terre - Switzerland

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.