I've seen an ultra suede dry matte glaze used on earthenware. Is it a custome recipe? Done in colors too.

Is it possible to get the same effect using other clays? See attached image.

Thanks in advance for any information on the topic.

MJ

 

 

 

post-2949-0-81505700-1446956997_thumb.jpg

Share this post


Link to post
Share on other sites

When I needed a stone matt glaze I found a glaze recipe that was close to what I needed and then reconfigured it to what I wanted. It took lots of testing (I bought a small test kiln) and patience.  It was a great experience in that I have the perfect glaze for my work and have a much better understanding of glaze ingredients and the make up of glazes. Read read read, test, test, test!

 

http://www.upenn.edu...book/14713.html  looks great!

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.