I have replaced the thermocouple several times in the 8 years I have had my Skutt 1027.  this last replacement, the kiln fired about 1/2 cone cooler. Never happened before. (Elements and relays are fairly new, a few firings on them. ) Any ideas why?

Share this post


Link to post
Share on other sites

When you say check it with cones,I think I did that. The cones in for the first firing with this new TC were one 5,the firing schedule I use normally gives me cone six. I need to run a glaze load tomorrow morning. I'm guessing and adding 10* to the peak temp with the same firing rate. I've got cones in, we will see. The 1/2 cone cooler left several of my glazes blah.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.