GGMS Posted October 23, 2015 Report Share Posted October 23, 2015 I once did ceramics in high school. I am trying to make a skip mold to make a specific soap dish. I tried making it myself, but it was not successful. Thanks Link to comment Share on other sites More sharing options...
oldlady Posted October 23, 2015 Report Share Posted October 23, 2015 a little more information about what you expect of us would be helpful. do you want instructions on making a mold of a specific thing to use for a soapdish? do you want general information on working with plaster? there are lots of things you could be asking. photos also help. Link to comment Share on other sites More sharing options...
Chilly Posted October 24, 2015 Report Share Posted October 24, 2015 Search from the main forums page for slip molds. there was a topic with lots of help, just a week or to back. Link to comment Share on other sites More sharing options...