bsalab714 Posted September 14, 2015 Report Share Posted September 14, 2015 I had crazing with all the clear recipes I could find or develop, with Insight Thermal Expansion at 6.55 or above. I have clear glazes working craze-free on Bmix, so I blended 50/50 (Calico/Bmix) and tried my suite of clear glazes. I fire both gas and electric to soft cone 7. Does anyone have a clear which does not craze over Calico? I am using Busch Nutmeg over this 50/50 blend, but that is the only one I have found to work, and seek other options. Link to comment Share on other sites More sharing options...