Nat Posted August 27, 2015 Report Share Posted August 27, 2015 I'm using silicon carbide to produce crater glazes, worked great in cone 6 but no result at cone 04. Is there any way to produce low fire crater glazes? Thanks Link to comment Share on other sites More sharing options...
Marcia Selsor Posted August 27, 2015 Report Share Posted August 27, 2015 here is an article from Ceramics Art Daily (upper left header) http://ceramicartsdaily.org/ceramic-glaze-recipes/low-fire-glaze-recipes/top-crater-glaze-recipe-cone-08-04-oxidation/ Link to comment Share on other sites More sharing options...
Min Posted August 27, 2015 Report Share Posted August 27, 2015 There is a ^08 - ^04 one in the CAD freebies section, "33 tried & true glazes" second edition. It's a base glaze with a top glaze combo, it's on page 5. From James Haggerty, Ceramics Monthly, November 2005 Link to comment Share on other sites More sharing options...
Nat Posted August 27, 2015 Author Report Share Posted August 27, 2015 Thank you both, will take a look. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.