Hi everyone. I just inherited 300 pounds of this clay. I've never used it before and was wondering if anyone has experience with it. I'm interested in anything unusual or weird that I should be aware of. Most of my experience lies with low fire earthenware and Cone 10 porcelain but very little with this type of stoneware. Thanks.

 

Paul

Link to comment
Share on other sites

http://www.sheffield-pottery.com/4DS-Moist-Stoneware-Pottery-Clay-Body-p/mc4ds.htm

 

Looks like a speckled brown clay. 

 

Shrinkage  c/6/ox./ 10.00%

Absorbtion c/6/ox./ 2.00%

 

It has good numbers. Seems fine. Glazes will be darker on it than your white clays. 

 

 

This post talks about 4ds:

http://community.ceramicartsdaily.org/topic/7246-your-favorite-clay-to-throw/?p=69176

Link to comment
Share on other sites

Thanks Grype. I actually did read that thread and searched google for all of the other information before posting. I'm trying to find out if there are any weird or unusual experiences that other forum members may have had.

 

Paul

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.