since the side will flux a glaze you could use something for ^2-3. You might find more for that range.You could try this one:

 

 

Wright’s Water Blue Glaze Cone 1-6 Oxidation

Glaze Material

Percentage

Lithium Carbonate 3%

Strontium Carbonate 9

Frit 3110 59

Edgar Plastic Kaolin 12

Flint 17

Total 100%

Add:

Bentonite 2%

Copper Carbonate 5%

 

 

Marcia

Share this post


Link to post
Share on other sites

You could try contacting Jack Olive on the Sunshine Coast in BC. His functional pots are all ^1.  He might be able to point you in the right direction for a ^1 glaze. (his functional pots are decorated with coloured slip then a clear glaze overtop)

Share this post


Link to post
Share on other sites

I used a combo of frit 3110, Epk and Bernard slip for ^1 soda on terra Cotta. 

http://community.ceramicartsdaily.org/gallery/image/3439-small-arch-terra-cotta-soda-fired/

 

 

 

 

 

 

This is a take off from Val Cushing's ^04 underglaze 

using 1/3 Frit 3110, 1/3 EPK and 1/3 stain.

 

birdman 2 copy.tiff

 

Marcia

birdman 2 copy.tiff

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.