I’m now a believer!  My experiment with a wood fired Raku kiln was a success thanks to the information and suggestions from knowledgeable people on this forum. 

I ripped apart an old electric kiln and used the ceramic fiber blanket surrounding the fire brick to build a light weight kiln. Since there was no breeze the day I fired, a squirrel cage fan was used to improve air flow.

Pictures show the kiln and results.   Oh yes, the marshmallows were great! 

post-67258-0-43157400-1439144515_thumb.jpg

post-67258-0-06908900-1439144761_thumb.jpg

post-67258-0-43157400-1439144515_thumb.jpg

post-67258-0-06908900-1439144761_thumb.jpg

Share this post


Link to post
Share on other sites
Guest JBaymore

 . . . but I'd not sure about roasting the marshmallows with a kiln constructed from an old fiber lining. 

 

And whatever ended up impregnating/contaminating the refractories in the old electric kiln.

 

best,

 

.......................john

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.