Couldn't you just mix up a ^10 slip, Robin Hoppers or Daniel Rhodes recipes come to mind, for damp ware and opacifiy it with zircopax? If the slip gets to refractory from the zirco then just add more flux to it. C&C for the ball clay part of the recipe and probably grolleg or epk for the kaolin part.