Can I write names on mugs with Mayco's Designer Liner over an opaque glaze once it's dry? 

Do I need to put clear glaze over the lettering?  Or over all? Does clear glaze over another glaze make them run?

 

Can I put the liner on a bisqued mug and then, when it's dry, apply a transparent glaze over it? Or a celadon? Will the letters show through?

 

Anyone know?

 

 

 

 

 

Link to comment
Share on other sites

I have used the green and the blue.  The colors are matt so if you want a shiny look you have to clear coat. I have hopefully attached two photos showing some things I have done.  Once it dries fully putting on an overcoat does not seem to smudge.  I have done a light green over it and it muted the colors but could still be seen.

post-58820-0-02270200-1434546777_thumb.jpg

post-58820-0-13495800-1434546836_thumb.jpg

post-58820-0-02270200-1434546777_thumb.jpg

post-58820-0-13495800-1434546836_thumb.jpg

Link to comment
Share on other sites

I have used the green and the blue.  The colors are matt so if you want a shiny look you have to clear coat. I have hopefully attached two photos showing some things I have done.  Once it dries fully putting on an overcoat does not seem to smudge.  I have done a light green over it and it muted the colors but could still be seen.

Good products! Nice detail!

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.