It adds some silica into the melt, and causes localized reduction within the melt. The outgassing can cause a lot of bubbles in the glaze, and it can be used decoratively for "crater glazes".

 

best,

 

.................john

Link to comment
Share on other sites

It adds some silica into the melt, and causes localized reduction within the melt. The outgassing can cause a lot of bubbles in the glaze, and it can be used decoratively for "crater glazes".

 

best,

 

.................john

 

 

 