jnapier Posted June 1, 2015 Report Share Posted June 1, 2015 Hi guys, I'm looking for anything that I can add to my porcelain slip (cone 10) that will result in a fine surface texture. This could be fairly uniform almost sandpaper-y, to just varied and rough. Like below: http://www.walkerceramics.com.au/images/Compressed%20images/BRT%201280%20R%20054.jpg http://claymotion.com.au/wp-content/uploads/2013/05/brtsample.jpg Not necessarily the colors I"m after, more just the texture, but open to any suggestions. Any thoughts would be great! Link to comment Share on other sites More sharing options...
oldlady Posted June 1, 2015 Report Share Posted June 1, 2015 molochite. Link to comment Share on other sites More sharing options...