Suggestions Needed For Colorants


Recommended Posts

I am testing the following glaze and would like it to be a bit more mint green, bluer side of light green. It is a great surface, but just a touch more yellow green than I am looking for. What changes do you recommend to get there? Add a 1/2 percent cobalt?

 

The base is the Calcium semi matt from MC6G.

3195 22.2

wollastonite 21

neph sy 4.4

EPK 33.3

silica 18.8

 

I added copper carb 1.50

rutile 7.00

 

With the same base and cobalt 1.0, titanium diox 3.0, I got a strong sky blue, not what I want either.

 

Thanks for any direction that will help me narrow down the testing, I am new at changing a glazes color.