I am testing the following glaze and would like it to be a bit more mint green, bluer side of light green. It is a great surface, but just a touch more yellow green than I am looking for. What changes do you recommend to get there? Add a 1/2 percent cobalt?

 

The base is the Calcium semi matt from MC6G.

3195 22.2

wollastonite 21

neph sy 4.4

EPK 33.3

silica 18.8

 

I added copper carb 1.50

rutile 7.00

 

With the same base and cobalt 1.0, titanium diox 3.0, I got a strong sky blue, not what I want either.

 

Thanks for any direction that will help me narrow down the testing, I am new at changing a glazes color.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.