Does anyone have a lowfire 04-06 aventurine glaze recipe that they would be willing to share? I have done quite a lot of searching on line and have not been very successful. Thanks so much in advance for your help.

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

Anne Currier Water Blue ^06

 

Frit 3110 73

 

Gerstley Borate 7

 

Silica 10

 

Kaolin 7

 

Zinc 3

 

Copper Carb. 4

 

 

 

 

Try this one.

 

 

Marcia

 

 

Share this post


Link to post
Share on other sites
PotsbyChar    0

Anne Currier Water Blue ^06

 

Frit 3110 73

 

Gerstley Borate 7

 

Silica 10

 

Kaolin 7

 

Zinc 3

 

Copper Carb. 4

 

 

 

 

Try this one.

 

 

Marcia

 

 

 

 

Thank you so much Marcia...will give this a try.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×