Does anyone have a lowfire 04-06 aventurine glaze recipe that they would be willing to share? I have done quite a lot of searching on line and have not been very successful. Thanks so much in advance for your help.
Pots by Char

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 5,484 posts
  • LocationBrownsville, Texas

Posted 14 May 2011 - 09:16 AM

Anne Currier Water Blue ^06

Frit 3110 73

Gerstley Borate 7

Silica 10

Kaolin 7

Zinc 3

Copper Carb. 4




Try this one.


Marcia



Marcia Selsor, Professor Emerita,
Montana State University-Billings

Marcia Selsor Studio in Brownsville, Texas.

http://www.marciaselsorstudio.com


#3 PotsbyChar

PotsbyChar

    Member

  • Members
  • PipPip
  • 27 posts
  • Locationcommerce texas

Posted 17 May 2011 - 07:57 AM

Anne Currier Water Blue ^06

Frit 3110 73

Gerstley Borate 7

Silica 10

Kaolin 7

Zinc 3

Copper Carb. 4




Try this one.


Marcia




Thank you so much Marcia...will give this a try.
Pots by Char