Jump to content

Search the Community

Showing results for tags 'nancy zoller pottery'.



More search options

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 4 results

  1. Nancy Zoller

    Pitcher

    From the album: Current work 2015

    Pitcher fired cone 10 reduction Glaze: Penland Celadon/Recipe C Tan/w red
  2. From the album: Current work 2015

    Hand Built Leaf Platter Fired cone 10 reduction Glaze: Recipe C Tan/Dark Blue Celadon layered
  3. From the album: Current work 2015

    Boat Shaped Olive dish w/rolled leaf pattern. Cone 10 reduction fired Recipe C tan/Dk. blue Celadon layered glaze.
  4. From the album: Current work 2015

    Large woven platter fired to cone 10 reduction glaze: Seafoam Green
×
×