Oh the joy of buying 15'' shelves, then getting home and they dont fit cause they are 15.5 inches and you have an L&L Kiln with element holders. DUN DUN DUN....
Mar 21 2017 12:21 PM
  • Babs's Photo
    Babs
    I can see the bright smile of satisfaction shining through the dust!
    Mar 23 2017 12:53 AM
  • oldlady's Photo
    oldlady
    what a shame that your nice pink respirator will turn very pale pink or even white!
    Mar 24 2017 10:38 AM
  • Joseph F's Photo
    Joseph F
    Whew... Done! Now I have blackish/grey kiln shelves. The corelite shelves held up a lot better than the cheap ones that I bought a while back. Those are like the ocean now. The corelite ones you can't even tell a grinder was on them. When I finished I patted my clothes off and it was a white dust storm. The sky was blocked and my dog yelped because she was scared of the sudden darkness.