Ten pounds of clay makes a rather large mixing bowl...the process may be justification for questioning my sanity :)
Jan 12 2014 04:37 PM
  • Rebekah Krieger's Photo
    Rebekah Krieger
    you must be mixing one hell of a batch of something… When I "over do it" with multiplying a bath too many times, I end up busting out the canning barrel. A 10lb bowl would come in handy here!
    Jan 13 2014 08:41 AM
  • Rebekah Krieger's Photo
    Rebekah Krieger
    *batch not bath

    Jan 13 2014 08:41 AM
  • ChenowethArts's Photo
    ChenowethArts
    rebbylicious, I am fortunate to have access to a large Soldner mixer and try to mix 150-200 pounds at a time. When removed in 10pound lumps, wedged, and bagged, that takes up most of a 50gal Rubbermaid trash container. For me, throwing 10 pounds is stretching my skill (and comfort) level...but I am getting there. Thanks for the notes, all!
    Jan 13 2014 09:32 PM