Spent all morning breaking up pallets and feeding the fire. We put last week's pots into altar fires, put the altar fires onto the embers of a big fire and piled wood on top, and kept on piling it on. Left it to die down and cool and wow, we had pots. Mine (the thinnest) broke but the thicker ones were fine. Everyone was delighted, now they want o play with real clay