Waiting for the over-watered home-made slip to evaporate........
Jun 13 2014 11:35 AM
  • Chilly's Photo
    Trouble is, it's not settling out. Still looks as it was when I finished mixing it. Now decanted into four buckets not two. Come on sunshine, do your stuff.
    Jun 14 2014 03:22 PM
  • Babs's Photo
    Add some dry clay trimmings, let slake and sieve again, aztest way to go. Add Flocculant?? Try somee epsom salts.
    Jun 14 2014 09:03 PM
  • Chilly's Photo
    I'm clean out of any more clay of that type at the mo. Patience is getting there. Daytime highs of 40C in a closed glasshouse......
    Jun 16 2014 04:38 PM