Jump to content

Community Status Updates


Rebekah Krieger

Just turned on a bisque load- this one contains little handprints on slabs for my sons preschool class, they are my first slabs and have already warped a lot, but I need to get them done before school lets out this year.
May 19 2014 05:00 PM
  • Rebekah Krieger's Photo
    Rebekah Krieger
    no - I just turned it on medium for a cone 05

    May 26 2014 09:16 PM
  • Benzine's Photo
    A little candling never hurt....
    May 26 2014 10:23 PM
  • Min's Photo
    Those closed forms seem to take forever to dry. Agree with Benzine about candling them.
    May 27 2014 05:59 PM