  1. Hi! I'm quite new to this forum and I'd like to ask your opinion. We had a glaze in the workshop which looks super awesome and I have no idea what it could be. I was thinking some of you might have an idea what components are used here. Or maybe you've already seen something like this before. Its dominant colour is that peach-green but the thicker parts turn purple. (these were all cone 6) https://i.ibb.co/4sdTZdG/Photo-24-04-2019-14-38-46.jpg https://i.ibb.co/7gwbfkg/Photo-24-04-2019-14-38-52.jpg https://i.ibb.co/G5KSnNN/Photo-24-04-2019-14-54-13.jpg
×
×