  1. Oops, I am a new potter and accidentally used Custer Feldspan instead of Soda Feldspar. What should I do? Thanks! cone 6 2000g Batch Gerstley Borate 634g Flint (Silica) 594g *asked for Soda Feldstar used Custer Feldspan 396g Talc 277g EPK 99g
×