  1. I am gonna try that it does look similiar to black iron oxide that I have.
  2. I have not used it in anything else. It is labeled cobalt oxide. One I worry the supplier messed up, and it wasn’t cheap.
  3. redart 56 whiting 29 strontium carb 10 frit 3195 5 cobalt oxide 1.3
  4. I am new to the community. My website is Eastwood Pottery I have a question regarding Hannah's Fake Blue Ash glaze. My glaze always comes out brown. I left out the RIO and just used the Cobalt Oxide but I still for the life of me cannot get blue. Does anyone out there have success using the blue ash glaze and do you use cobalt oxide as in the recipe?
×
×