  1. Making terra cotta bricks

    Triolaz, thanks, do you have the proportions of redart/sand/ball clay that he uses? Pete
  2. Dear all, i want to carve some bricks while they are soft, then sun dry them, then fire them extra slowly, then carve the detail into the well fired brick. I've researched this and all the instructions tell me to dig up natural clay. I can't do this as i live in the city and i don't have land to dig. Would it work if i buy some terra cotta powder and silica sand, add water, and mix it thoroughly? Regards, Pete
×