  1. I read the other posts about this, I find my situation to be different because I don't plan on using them again with wash, I just want to keep them clean. The other posts recommended the same method of cleaning, I wanted to know what harm there is in using water, even if I let them dehydrate for a significant period.
  2. Hi. I bought a used kiln, and it came with 6 shelves. All of the shelves have kiln wash on them that is cracking and falling off, and leaving white powder everywhere. There is no glaze on the shelves at all. Could I clean them off by pressure washing them and letting them dry ? Or will this pwrman damage them? I want them clean because I do not ever plan on using glaze, so I want them to be free of the kiln wash. Thanks!
×

Important Information

By using this site, you agree to our Terms of Use.