    Raku, Barrel and saggar firing. Looking for a pottery surface that creates a "mysterious presence" which the viewer can experience.
  1. Low-fire beaded glaze

    Hello- I'm looking for a low fire beaded/crawling type of glaze. This glaze will be raku fired and pretty much a base that can accept any variety of colorants. Anyone care to share something on this order? Thanks for any help!
  2. Barrel Fired Pots

    Pots which were barrel fired. All work was burnished and sprayed with Terra Sigillata, then fired with mixed hardwoods in a steel barrel along with color carbonates, salts and other organic materials.
  3. Barrel Fired bottle

    From the album Barrel Fired Pots

  4. Raku

    Raku pots I've created.
  5. Gold Leaf Raku Jar

    From the album Raku

  6. Barrel fired form

    From the album Barrel Fired Pots

  7. Barrel Fired bottle form

    From the album Barrel Fired Pots

  8. Barrel fired form

    From the album Barrel Fired Pots

  9. Barrel fired form

    From the album Barrel Fired Pots

  10. Large Raku Driftwood handled piece

    From the album Raku

    23" Tall Raku fired form with driftwood handle. Copper matte glaze. Raku fired and smoked in newspaper and sawdust for reduction.
  11. Stretched Raku Jar

    From the album Raku

    Raku Fired Jar with lid. Stretched with sodium silicate. Multiple layered glazes. Raku Fired with sawdust and newspaper for reduction.
  12. Barrel fired Bottle form

    From the album Barrel Fired Pots

    15" Tall barrel fired bottle.
  13. Saggar fired Bottle

    From the album Raku

    Sagger fired bottle form. 13" tall.
  14. Maple Leaf Raku Vase

    From the album Raku

    22" Tall. Carved maple leaf pattern, multiple glazes. Raku fired and reduced on sawdust bed.
  15. Wisteria Raku Vase

    From the album Raku

    20" Tall, burnished and raku fired-reduced on sawdust bed.
×