  1. Good morning, I am new to electric kiln firing and as such kiln wash. Bought some that was mixed from a local studio and applied 3 coats. First one may have been a little thick so I thinned up the latter coats. After drying each layer I have noticed some cracking on the surface. What should I do ? Should I sand it till no longer visual. It is sparatic on some but not all of the shelves.

    Planning on doing a bisque fire soon.

    Thanks so much for help !!

×
×