Posts
5,838 -
Joined
-
Last visited
Min's Achievements
Advanced Member (3/3)
6.3k
Reputation
Single Status Update
-
Min I don't think I took any photos of the dishes, I was working at my store 70 to 90 hours a week and made the dishes when I had a moment to spare. My friend wanted a entire formal place setting so her daughter didn't have to eat off of plastic dishes at family dinners and holidays. I made the entire formal place setting including cups and saucers, they were mostly for looks. I believe I made the soup bowl with no rest on it. I can tell you that I had a lot more curve inward at the top edge and it curved further around. The had rest was added to the lowest side of the curve. A half round shape, my friend wanted it so her daughter couldn't flip the dish when she laid her arm down. She couldn't gently lower her arm. Can the lady you are making it for try it out? Denice