  1. Porcelain

    Hey guys I'm new to the forum, though not new to potting. In response to your question, I would highly recommend Coleman Porcelain by Aardvark Clay. It is a good throwing body, though it is not the most translucent porcelain in the world, if that's what you're after. I throw with it regularly and don't have any trouble. It is a ^10 clay.
×