  1. Re: Friedl Holzer-Kjellberg's work ... can I just say WOW!!!!!!!!!

    I would call that mastery of form and glaze ... incredible learning curve ... not for the feint of heart.

    I am totally green with envy and wondering if I should make myself crazy by trying it at least once.

    Does anyone have a nice Cone 6 clear recipe?

    biggrin.giftongue.gifrolleyes.gif ... just kidding.

    This is a Harry Memmott cone 6 clear glaze..good with underglazes and lustres and best of all...three ingredients!

    Kaolin 15

    Silica 35

    Gerstley Borate 50

    Let me know if you like it.

×
×