  1. I have two cone 04 clear glazes that I am trying to eliminated crazing from. 1st glaze formula- Gerstley Borate 25 Ferro Frit 3124 25 Soda Feldspar 20 Cornwall Stone 20 Whiting 5 zinc Oxide 5 2nd glaze formula- Gerstley Borate 26 Lithium Carbonate 4 Ferro Frit 3124 30 Neph Sy 20 EPK 10 Flint 10 Clay Body- Tile #6 30 Neph Sy A400 25 KT om4 Ball Clay 20 Holmes Fredeick Fireclay 15 Cedar Heightd Fireclay 10 Any Suggestion? Thanks
×