  1. Use Of Gum Of Arabic With Clay

    Peter, Thank you so much for the information. I will definitely try this. Patty
  2. I recently toured the Belleek factory in Ireland and found that they use gum of arabic in their clay body to be able to make those delicate and intricate basket forms. The gum of arabic apparently allows the clay to be more pliable and not crack while forming the basket shape. Does anyone know the process and proportions for adding gum of arabic to clay for this purpose?
×