  1. Like
    Bobg got a reaction from Lucille Oka in Looking For Underglaze?   
    I'm looking for an underglaze that will give me the same color as in the picture at cone 6.  Any one have a clue where I can get some?  I'd even be interested in a glaze.
     
    Bob


  2. Like
    Bobg got a reaction from SmartsyArtsy in Tomato Red glaze.   
    i'm looking for a tomato red ^6 glaze that I can buy. I don't have the time right now to be mixing one up. I know Seattle Pottery Supply offers one, has anyone used it. Looking for other source and would appreciate any help I can get.
     
    Thanks,
    Bob
  3. Like
    Bobg got a reaction from Smallshapes in Firing electric kiln in wooden shed   
    Skutt recommends at least 18 inches. I leave my garage door open slightly so the fumes can get out. I fire my Skutt 181 on a cement floor on the factory stand that is on a wooden dolly. The wood doesn't get hot at all and I don't worry about it.
     
    Bob
  4. Like
    Bobg got a reaction from Spring Mold in Recipe For Neat Oxides   
    I just take some of the the clay I'm building pots out of, put it in a blender with a little water. Process it until you get to the thickness you like, I make mine almost like pudding. I then add a certain percentage of oxide and you'll have to play with this. I mix 5% cobalt for my blue items.
×
×