    Coloured Slips

    I dont mind seeing the traces of process
  2. mitch72

    Coloured Slips

    You want to be looking up vitreous slips. Plenty of recipes for your relevant temp.I've used some, but not currently. TJR. Yeah I thought vitreous slips might be the ticket. Do they give a different surface than spaying a thin layer of frit?
  3. mitch72

    Coloured Slips

    Im hoping for some suggestions on how to improve the colour intensity of coloured slips (without using a shiny glaze) I want to achieve the (wet stone look) Ive always worked with sigilattas which im drawn to for there surface texture. So im wanting to get a similar surface whilst using coloured stains?
×