  1. most iridiscent effect

    dark brown clay body with thick red iron oxide wash after bisquing... comes up a nice silver
  2. cone 10 shino, no crawling

    I live and die by Steve Loucks' carbon trapping shino... rich reds, lusterous tan, crystallized green (according to thickness of application.) Steve Loucks Shino Neph Sy - 45 Spodumene - 15 OM-4 - 15 F-4 feldspar - 10 Red Art clay - 5 ---------------------- Soda Ash - 18
  3. Questions about Iron Oxide & Nepheline Syenite

    i toss in ferro frit 3124... same effect.
  4. ^4-6 metallic gold glaze

    no problem... i will look for that issue in my library's data bases!
  5. ^4-6 metallic gold glaze

    thanks for the link and the heads up... i always pay attention to what ron roy has to say!!!
  6. ^4-6 metallic gold glaze

    now you have piqued my interest... do you know off-hand if ceramics review archives back issues on line?
  7. anyone have a good recipe for a cone 4-6 metallic gold glaze? thanks!
  8. i'm a hand builder, and i normally listen to things that make me dance around the studio; i listen to a lot of chris cornell, primus, led zepplin, tori amos. every activity in a studio had a specific dance that goes along with it!
  9. i know what i am going to play with this summer....
  10. Verdigris Glaze

    i use this cone 6 glaze all the time... tried and true TurquoiseNeph SyStrontiumFlintBall ClayLithiumTotal Also add:Copper CarbBentoniteEpson SaltComments:Very bright. Very turquoise, Matt, breaks black. Moves a lot if applied too thick. Create rough antique look a like texture.
  11. Gloss White ^6 Ox

    Ruth, I haven't tested this glaze but I remembered reading about it that is was a simple glaze to make. It's Tony Hansen 5X20 plus 10% zircopax White Gloss here's the formula 20-Frit 3134 20-EPK 20-Silica 20-Custer Spar 20-Wollanstonite 10-Zircopax. I read a review of a test by Alisa in Denmark, she said that Cobalt, RIO, Black Stain. Chrome and Yellow Ochre showed well under the glaze held their edge and stayed exactly as painted. Test away! i tested this... pretty nice glaze, a bit of streaking. for the most part, useful (especially for students.) thanks again!
  12. Gloss White ^6 Ox

    Ruth, I haven't tested this glaze but I remembered reading about it that is was a simple glaze to make. It's Tony Hansen 5X20 plus 10% zircopax White Gloss here's the formula 20-Frit 3134 20-EPK 20-Silica 20-Custer Spar 20-Wollanstonite 10-Zircopax. I read a review of a test by Alisa in Denmark, she said that Cobalt, RIO, Black Stain. Chrome and Yellow Ochre showed well under the glaze held their edge and stayed exactly as painted. Test away! a thousand thanks! i'll let you know how it tests out.
  13. Orange glaze cone 6 >46.7 Potash >4 Kaolin >2 Bentonite >15 Bone ash >4 LIthium Carb. >16.9 Talc >11.4 Silica >10 RIO Gloss surface glaze that covered well. Nodiscernable difference where dipped twice. It is a rich, medium brown with very vivid orange streaking throughout. Surface is fluid but not runny. The orangesare very bright. Variation: added 10 Ochre Same base color, but no orange streaking. Insteadthe glaze has a creamy yellow cast where thickest.
×