  1. I don't know if it exists in your country, but if you find it the best is IN2210 from RUBSON (but it stinks a lot during few days) or if you don't have glaze inside of the vase you can use IN2230 from RUBSON. For both of them you let the product in the vase for 10 minutes about, then you let it dry few days and it will be waterproof... Laurent(sorry for my very bad english)
×