  1. I absolutely love this glaze and has become a favorite of my clients. The problem that you are having is that you are not applying it thick enough. When I make or purchase a new glaze I always run a test piece putting rings of glaze starting with one coat at the bottom and then two, three and four, I top it off with a thick rim to get a drip break. What I found is that to get a more solid red you need to apply four heavy coats, if you only apply three coats then you get the dark almost black look. What I prefer is to apply three even coats and then apply a mottled coat so that some of the darker breaks come through, see attached picture. I fire to cone 6 oxidation. Mark
×