Jump to content

mudpups

Members
  • Content count

    1
  • Joined

  • Last visited

  1. I found a thread about this where someone gave a recipe - something like; 1 part stain, 1 part frit, 1 part bentonite. I kept the page open, went out to walk the dog, came back to get the recipe to make it and my computer had crashed - do you think i can find that thread again! NO! Please, what was the recipe to turn a stain into an underglaze?
×