  1. I’m an amateur, and it shows.

    Thank you all for the advice. Next time I am doing something I have never done before, I will defiantly test before I proceed. Thanks again.
  2. I was hoping someone would be ableto give me some advice. I usually only use my kiln for green ware firing andglazing. This was my first attempt at over-glaze. I fired my bisque to cone 04and glazed it with gloss glaze to cone 06. I bought a bottle of Colorobbia goldand the clerk told me to brush it on and fire to cone 018. I think I missedsomething. I’m not sure if I didn’t apply enough, I applied to much, the conewas too hot / too cold, or the gloss glaze was the wrong type. What did I dowrong? Also, if anyone can tell me how I can fix the 30 pieces that I ruined itwould be greatly appreciated. Please see attached pictured.
×