  1. Glaze Calculator

    Agni, There are many programs available, some free. Glazemaster is a database program, $50US, for Mac or PC that I have found easy to use. http://www.masteringglazes.com/Pages/GM1frame.html Insight, as others mention, is very good, costs a bit more. Hyperglaze, by Richard Burkett, at the U. of San Diego, US, is written by an artist and seems less linear to me, cost $100US, is a full-featured program. www.hyperglaze.com
×