  1. temp for opening kiln?

    Hi Ginny, I have an L & L with a computer. I always do a slow bisque and a slow glaze, I leave the top plug out and I do a 5 minute hold on the glaze. So far this works great. I also make sure my greenware is real dry, I can tell by the weight when I pick it up. If I get in a hurry or I think its good and dry by its not, I have had some blow ups - not pretty!!
×