  1. Hi everyone from Sunny Ireland!

    Im hoping someone can help before I ruin another load of work!

    Pot on the left is what I am trying to achieve, it was a happy accident as I just wanted to fill a space. I think I put a thinish layer of Copper Carbonate on then a layer of transparent glaze and fired to cone 05. Delighted with the colour I tried to repeat it, 

    Pot in the middle has a thick layer of the same , my thinking was it would be even more blue, it wasnt!!

    The next item was treated the same and the transparent glaze seems to have crazed and cracked and is a nasty colour , the final item had no transparent glaze on it , again black/brown colour.

    How can they be so different?  Was it because I put a thick layer on and why would the transparent glaze react that way?

    I know there will be someone in this community who can help, Thanks So much, Jools

    IMG_6440.JPG

×
×