  1. Maybe another question you should be asking is, "How do you know what the customer will use the bowl for" maybe use only food safe in all items which COULD be used for food. Maybe the Fruit bowl for examle, might be used for Salad.
  2. Im still looking for some kind poerson to give me a reliable recipe for a WHite Glossy Glaze. Body is Earthenware and maybe Terracotta, Fired to 1080 electric. Glaze should be functional ( food safe) Regards To All
  3. Did I get ripped off?

    If it does what you want to do, then be happy, Theres no milage in looking over your shoulder.
  4. Blood pressure 150/75

  5. I asked a while ago for a recipe for white and clear glaze. Clay is earthenware white, temp is 1080C Any ideas ? Thanks
  6. Pugmills

    does the Mill have a fine filter, Does it have a vacuume system to remover air when pugging. Regards
  7. Tissue Transfer?

    Thsi is NOT Slip. Its Images and or patterns on Tissue paper.
  8. Not Using Kiln Wash?

    Why would you not use kiln Wash ?
  9. Frit 3134 2100 grams Ball Clay 378 Zircon Flour 378 Fire to 1000c - 1080c When you rech temp spray with find water, then reduce with paper or sawduse for 30min When cooled re-heat to say 100-150 to open the cracks then use strong tea, coffee or anything dark to empasise the cracks. I have used this recipe many times. Regards
  10. Tissue Transfer?

    ive searched and found nothing Google only comes up with pre printed or the sliding type transfer. Thanks
  11. Clear Glaze - White Glaze

    White Earthenware, 1080C electric
  12. Anyone got a reliable EARTHENWARE recipe for a Clear Glaze and a White Glaze. Both for functional wares. Thanks
  13. Tissue Transfer?

    Have tissue and wish to print an image or text onto it. Then transfer this onto the clay ? Ok, how do I preint the image onto the tissue, Prefer Printer if possible. Any ideas on the type of Ink??? Regards