  • IMG 0002
    IMG 0002
    I stuck the Colemanite in a bisque firing to 915 C, which should be around cone 09. Theoretically, Colemanite has an LOI of 21.9%, but I've seen an analysis of 23.7%. I don't have the exact % weigh...
  • IMG 0002
    IMG 0002
    Pieter:When I have chemically etched materials they separate out into carbons, solids, and metals. I would agree soluble salts are clinging to the sides: but by chance are those carbons floating? I...
  • IMG 0002
    IMG 0002
    This is just calcined Colemanite in some water in a polystyrene cup. See my post in this thread for more context:http://community.ceramicartsdaily.org/topic/15955-colemanite/ I think the light...
  • TLH SYOM 33 NO4
    TLH SYOM 33 NO4
    I just added a pic with the stamp, which I had forgotten to do. The color of the piece is accurate in this view-looks too pinklish in the other pic.
  • Celadon
    Celadon
    Very nice. Can you add some close-ups, please? Nice form and fluting.