    Two firings, very slow bisque to cone 06, care at 212, 500 and slow transition at quartz conversion.
  • imageclose up
    imageclose up
    1100-1300F requires an oxidation atmosphere to burn off carbons. Did you once fire by chance?
  • imageclose up
    imageclose up
    No pinholes on the exterior, only on the inside.
  • imageclose up
    imageclose up
    Glaze is Malcolm Shino from the Brit book fired w/1hr Heavy reduction starting at 1540f and then medium reduction until cone 10 , R1 firing from the Britt book, on soldate 60.
  • imageclose up
    imageclose up
    Commercial premix or custom mix body? Glaze is littered with pin holes as well.